21 August 2026
Firing log: the August kiln
Twelve hours at 1240 degrees, then two days of waiting. What came out, what cracked, and why the ash bowls went darker this time.
Pieces from this firing
We loaded on Monday evening: forty cups, the last of the plates and six large bowls at the bottom, where the heat is most even. The kiln reached temperature by noon on Tuesday and we let it cool until Thursday.
Two cups cracked at the rim, which is normal for this batch. The ash bowls went a shade darker than in June, because the wood ash this time came from the neighbours' beech, not from the oak.